Why Medical Buyers Specify Grade 23 (Ti-6Al-4V ELI)

A Grade 5 certificate does not tell an implant buyer what an implant needs. Grade 23 is specified because oxygen is capped lower, chemistry is judged against ASTM F136 rather than ASTM B348, and every heat keeps its own paper. Only the first of those shows up on a price list.

Oxygen and the ELI Limits

ELI stands for extra low interstitial, and oxygen is the element that does the work. It strengthens titanium by sitting in the lattice. In a 3 mm (0.12 in) bone plate that a surgeon bends once on the table, that extra oxygen is the difference between a bend and a crack.

ElementGrade 5 max (B348)Grade 23 max (F136)What it does to a part
Oxygen0.20%0.13%Solid-solution strengthening; high oxygen lowers ductility and toughness
Nitrogen0.05%0.03%Strong strengthener; a small excess shows up as lost elongation
Carbon0.08%0.08%Same limit in both grades; not the ELI differentiator
Iron0.30%0.25%Residual from scrap and melting; beta stabiliser
Hydrogen0.015% (150 ppm)0.0125% (125 ppm)Hydride formation and delayed cracking under sustained load

Limits follow the current ASTM F136 and B348 text for bar. The edition on your purchase order governs. Tensile minimums move the other way: 860 MPa tensile and 795 MPa yield for Grade 23, against 895 and 828 for Grade 5, because less oxygen means less strengthening. Buyers accept 35 MPa less strength for ductility. A Grade 23 certificate that reports Grade 5 strength is a prompt to read the chemistry.

F136 Against B348

ASTM B348 covers titanium bar and billet for general engineering, while ASTM F136 covers wrought Ti-6Al-4V ELI for surgical implants; ISO 5832-3 is the ISO counterpart to F136. Chemistry is close to harmonised in current editions, which is why mills issue one heat against both documents. The documents themselves stay separate, and a notified body wants the standard the device was qualified to, named exactly.

Two consequences follow. A certificate reading "Ti-6Al-4V ELI, ASTM B348" answers a different question than "ASTM F136" and is not equivalent on an implant drawing. And if a customer needs ISO 5832-3, say so at inquiry stage. Dual-certified bar is routine, but it is arranged at the heat rather than added at the loading dock.

The Record Chain

Implant traceability is a chain of records from melt to device lot. It breaks at the weakest link.

StageWhat must be recordedWho holds it
MeltHeat number, actual chemistry including O, N, H, C, melt methodMill
Conversion to barHeat number carried through forging, peeling and grinding; no mixed heats in a bundleMill or converter
TestTensile and hardness per heat; O, N and H by inert gas fusionMill laboratory
DispatchHeat number against every bundle on the packing list, MTC to EN 10204 3.1Supplier
Incoming goodsPMI of alloy identity, count against the packing list, quarantine until releaseDevice maker

Where the Chain Breaks

  • Straightening or peeling done off-certificate. A subcontractor that re-marks bar with a lot number instead of the heat number has broken the chain.
  • One test standing in for two heats. A 4 t heat split into two conversions needs chemistry per heat, not per shipment.
  • Certificates with typical values. "Typical 0.11% O" is not a maximum and not a result, so ask for the actual analysis of your heat.
  • PMI mistaken for chemistry. Handheld XRF reads aluminium and vanadium and cannot see oxygen, nitrogen or hydrogen; only the mill's inert gas fusion proves ELI. A passing PMI is not ELI verification.

Purchase Order Lines

A Grade 23 line item that can be quoted without email traffic carries the standard and edition (ASTM F136, plus ISO 5832-3 if the file needs it), the condition, and diameter with tolerance, where ground to h9 is usual below Ø25 mm. Length and cut tolerance come next, then surface with alpha case removal stated, the test set per heat, and the marking method, since laser marking on the bar end is often a customer requirement. Close with a no-substitution clause naming Grade 5 as unacceptable.

Our Grade 23 medical titanium bar is supplied to ASTM F136 in the ground and polished conditions instrument and implant shops use, with chemistry reported per heat. Where a part is strength-limited and not implantable, Grade 5 titanium bar to ASTM B348 is the lower-cost answer, and the ASTM and AMS standards guide sets out which document covers which form. Certificate options sit on the documents and certificates page; the medical applications page covers instrument and implant duty.

ELI bar is a thinner market than Grade 5. Ground bar in the Ø6–32 mm (0.24–1.25 in) band used for screws, plates and instruments is normally available from stock in the Baoji–Xi'an cluster; larger diameters come from forging stock on a longer clock. Expect a premium for the tighter chemistry and extra testing, on request, and a lead time driven by diameter more than tonnage: on request.

Drawing and Certificate Chain

Send the part drawing or the bar specification, the standard and edition, and the traceability your quality system needs. We will quote Grade 23 to ASTM F136 with chemistry per heat, and say which documents travel with the bars.

Request a Grade 23 Quote

CATEGORIES

CONTACT US

Contact: Jessie

Phone: +86-19539017809

E-mail: sales@gktitanium.com

Add: BLOCK A, HUIHANG PLAZA , HANGTUO ROAD, NATIONAL CIVIL AEROSPACE INDUSTRY BASE, Xi'an