Titanium wire from Ø0.1 mm to Ø8 mm in Grades 1 to 4, Grade 5, 7, 9 and 12 to ASTM B863. Welding wire and filler rod ship from stock. Fine wire is drawn to order. Both are judged on diameter consistency and what is left on the surface.
The catalog splits in two, and the split follows the buyer rather than the mill. A fabrication shop orders by AWS class, diameter and spool type. A component maker orders by temper, tolerance and surface, because the wire is about to be formed, woven or fed into a head.
Request a Wire Quote Download Wire Size List
Welding wire and rod
Spooled wire for orbital, robotic and manual GTAW or plasma, vacuum annealed at final size and bagged with desiccant. Layer wound, because a crossed turn stalls a feeder two hours into a run.
AWS A5.16 · ASTM B863 · Ø0.8–3.2 mm · 1–15 kg spools
Cut lengths for hand TIG, end-stamped with grade and heat number, colour banded, sealed in capped tubes. Same drawing line as the spooled wire, then straightened.
AWS A5.16 · Ø1.6–4.0 mm · 1 m / 1.5 m · colour-coded
Fine wire and coils
Diamond-die drawn in Grade 1, 2, 5 and 9, annealed or cold worked to a quoted tensile range. Degreased and ultrasonically cleaned, with the cleaning route on the record.
ASTM B863 · Ø0.1–1.0 mm · ±0.005–0.02 mm · 0.1–5 kg spools
Layer-wound coils from 0.5 kg to 15 kg on DIN 100/200 or EN ISO 544 spools, or spool-less, wound under controlled tension to a set cast and helix.
DIN 100 / 200 · EN ISO 544 S100–S300 · 0.5–15 kg
Grades and classes
| Grade | UNS | AWS A5.16 | Rm min (MPa) | Typical wire use |
| Grade 1 | R50250 | ERTi-1 | 240 | Soft joints, mesh |
| Grade 2 | R50400 | ERTi-2 | 345 | Chemical plant, TIG |
| Grade 3 / 4 | R50550 / R50700 | ERTi-3 / ERTi-4 | 450 / 550 | Higher-strength CP |
| Grade 5 | R56400 | ERTi-5 | 895 | Aerospace, pressure parts |
| Grade 7 | R52400 | ERTi-7 | 345 | Reducing acid service |
| Grade 9 | R56320 | ERTi-9 | 620 | Tube work, eyeglass wire |
| Grade 12 | R53400 | ERTi-12 | 483 | Hot brine, crevice corrosion |
| Grade 23 | R56407 | ERTi-23 | 860 | Implant and cryogenic |
Tensile minimums follow ASTM B863 for the diameter and condition ordered. B863 governs the wire; AWS A5.16 governs the filler class. Ordering to one and expecting the other is the mix-up we see most often. How the two line up.
Diameter and coil weight
| Diameter band | Tolerance | Rm min (MPa) | Standard coil / spool |
| Ø0.1–0.5 mm | ±0.005–0.01 mm | Gr1: 240 | 0.1–1 kg spool |
| Ø0.5–1.0 mm | ±0.01–0.02 mm | Gr2: 345 | 1–5 kg spool |
| Ø1.0–2.0 mm | ±0.02 mm | Gr2 345 / Gr5 895 | 5–15 kg spool or coil |
| Ø2.0–3.2 mm | ±0.02–0.03 mm | Gr2 345 / Gr5 895 | 5–15 kg, or straight |
| Ø3.2–8.0 mm | ±0.03–0.05 mm | Gr2: 345 | 10–25 kg coil, or rod |
These bands are typical supply, not a specification. Final diameter, ovality and coil weight are fixed against B863 and the order. Diameter is gauged at both ends of every coil, because a spool that starts at the top of the band and finishes at the bottom changes the arc without warning.
Drawing and cleaning
Rod enters at Ø5.5–8 mm, pickled and inspected. From there the wire goes through blocks of passes: carbide dies down to Ø1.0 mm, diamond below. Ductility runs out after a few passes, so the wire is vacuum annealed between blocks and once more at finished size. That last anneal is the one that matters for hydrogen. Lubricant and moisture go in at the die, and the finish anneal is what takes them back out.
After drawing comes alkaline degrease, ultrasonic clean, deionized rinse, dry, spool. Residue that survives shows up later as porosity in a weld, or as outgassing under vacuum. It is not visible on the wire, which is why the test has to be on the record instead.
Inspection
| Item | Detail |
| MTC | EN 10204 3.1: chemistry, mechanicals, hydrogen, heat number |
| Dimensional | Diameter and ovality at both coil ends, recorded against the label |
| Surface | Slivers, die lines, staining; PMI and third party on request |
Packing and lead time
| Item | Detail |
| Spool | Vacuum bag, desiccant, carton or returnable shell |
| Coil | VCI film, desiccant, ISPM-15 case, foam |
| Straight rod | Rigid tube, capped ends, grade and heat on the label |
| Stock lead time | on request |
| Drawing lead time | on request |
| Minimum order | on request |
FAQ
Which wire for TIG on Grade 2 sheet?
ERTi-2 matches Grade 2 base metal. If the joint is formed after welding, ERTi-1 gives more ductility at a small strength cost.
AWS A5.16 or ASTM B863?
Both. A5.16 fixes filler class and chemistry, B863 the wire product and its properties. A PO quoting one usually needs the other behind it.
Lower hydrogen maximum?
Often, when the mill can vacuum anneal to that limit. Give the number in ppm and we confirm before the lot is booked.
Smallest diameter?
Ø0.1 mm in Grade 1 and Grade 2, drawn to order. Below Ø0.2 mm it is quoted per spool, because the drawing yield, not the metal, sets the price.
Quote
Send the AWS class, diameter, coil weight, process and base metal. For a critical joint add the WPS and the hydrogen limit, because those two decide the mill lot.
Request a Wire Quote