Titanium welding wire to AWS A5.16 ERTi-1, ERTi-2, ERTi-5 and ERTi-23, Ø0.8 to 3.2 mm, on spools, layer-wound coils or straight lengths. Drawn,…
Titanium welding wire to AWS A5.16 ERTi-1, ERTi-2, ERTi-5 and ERTi-23, Ø0.8 to 3.2 mm, on spools, layer-wound coils or straight lengths. Drawn, degreased and vacuum annealed at final diameter. Hydrogen is reported as a number on the certificate, not as a pass.
| Class | UNS | Base metal | Rm min, annealed | Typical joint |
|---|---|---|---|---|
| ERTi-1 | R50250 | Grade 1 | 240 MPa | Soft welds, linings |
| ERTi-2 | R50400 | Grade 2 | 345 MPa | Chemical plant |
| ERTi-5 | R56400 | Grade 5 | 895 MPa | Aerospace, pressure parts |
| ERTi-7 | R52400 | Grade 7 | 345 MPa | Reducing acids |
| ERTi-23 | R56407 | Grade 23 | 860 MPa | Implant and cryogenic |
AWS A5.16 fixes the class and the chemistry. ASTM B863 fixes the wire product and its properties. A tighter oxygen or iron limit than either standard asks for goes on the inquiry, in numbers, because the mill will not infer it.
| Ø mm (in) | Tolerance | Rm min, MPa | Spool / coil |
|---|---|---|---|
| 0.8 (0.031) | ±0.02 mm | 345 / 895 | 1 kg, 5 kg |
| 1.0 (0.039) | ±0.02 mm | 345 / 895 | 1 kg, 5 kg |
| 1.2 (0.047) | ±0.02 mm | 345 / 895 | 5 kg, 15 kg |
| 1.6 (0.063) | ±0.02 mm | 345 / 895 | 5 kg, 15 kg |
| 2.4 (0.094) | ±0.03 mm | 345 / 895 | 15 kg, or straight |
| 3.2 (0.126) | ±0.03 mm | 345 / 895 | 15 kg, or straight |
Tolerance covers diameter and ovality together, and both are measured at each end of the coil. A spool that starts at the top of the band and finishes at the bottom will move your arc voltage over a long run and there is nothing on the label to warn you.
| Item | Detail |
|---|---|
| Surface | Bright, bright annealed or pickled; no copper flash, graphite or soap film |
| Hydrogen | Stripped by the final vacuum anneal and reported on the MTC — on request |
| Packing | Vacuum bag with desiccant, opened at the feeder |
| Storage | Dry cabinet, used within on request |
| Handling | Clean gloves; bare hands leave chloride and oil |
Moisture is the quiet one. Wire that looks dry can carry a film that dissociates in the arc, and a spool opened on Friday and left on the bench is a porosity claim by Monday. The bag is part of the specification, not the packaging.
DCEN for GTAW, argon at 99.999% with a dew point of −40 °C or below, trailing shield above about 3 mm of plate. Keep the hot end inside the gas until it stops glowing, cut out any run where the tint turns blue or grey, and keep one cutter and one brush for titanium only. Straw colour is acceptable on most work. Blue is not, and grey means the shield was gone.
| Item | Detail |
|---|---|
| MTC | EN 10204 3.1, chemistry, mechanicals, hydrogen, heat number on the spool label |
| Dimensional | Diameter, ovality and surface recorded per coil |
| Extra | PMI or third-party inspection on request |
| Item | Detail |
|---|---|
| Spool | Vacuum foil bag with desiccant, carton or returnable shell |
| Stock lead time | on request |
| Drawing lead time | on request |
| Minimum order | on request |
ERTi-2 or ERTi-5?
Match the filler to the base metal. ERTi-2 for Grade 2, ERTi-5 for Ti-6Al-4V. A mismatch either weakens the joint or makes it brittle, and neither shows until the part is tested.
What hydrogen level can you hold?
The standard chemistry limit applies unless you specify otherwise. A tighter maximum is possible on vacuum-annealed lots, when the mill has the pump capacity for it.
Same wire on TIG and plasma?
Same class, same diameter. Plasma with hot wire feed needs a consistent cast and helix, so tell us the process when you order.
Send the AWS class, diameter, spool weight, process and base metal. A WPS or a hydrogen limit decides the mill lot.
Send Your Requirement · all wire and coils
Contact: Jessie
Phone: +86-19539017809
E-mail: sales@gktitanium.com
Add: BLOCK A, HUIHANG PLAZA , HANGTUO ROAD, NATIONAL CIVIL AEROSPACE INDUSTRY BASE, Xi'an