Grade 7 (Ti-0.2Pd) and Grade 12 (Ti-0.3Mo-0.8Ni) bar exist for the services where Grade 2 does not hold: reducing acids, hot chlorides, crevices…
Grade 7 (Ti-0.2Pd) and Grade 12 (Ti-0.3Mo-0.8Ni) bar exist for the services where Grade 2 does not hold: reducing acids, hot chlorides, crevices under gaskets. Both keep titanium's seawater behaviour and push it into hydrochloric, sulfuric and organic acid duty. We supply Ø10–250 mm bar to ASTM B348.
Commercially pure titanium lives on a passive oxide film. In oxidizing conditions the film repairs itself within milliseconds. In reducing acids, hydrochloric below a few percent, hot sulfuric, some organic acids, it does not, and attack starts in gaps and under deposits where the oxygen supply is thin.
Palladium, 0.12–0.25% in Grade 7, lowers the hydrogen overpotential at the surface and keeps the film repassivating. Pd is expensive, which is why the same chemistry appears as Grade 11 in plate and sheet. Grade 12 takes another route: 0.3% molybdenum and 0.8% nickel strengthen the film and lift the crevice-corrosion temperature at about half the cost of a Pd grade.
| Condition | Grade 7 (Ti-0.2Pd) | Grade 12 (Ti-0.3Mo-0.8Ni) |
|---|---|---|
| Hydrochloric acid, dilute to moderate | Preferred | Limited |
| Sulfuric acid, reducing | Preferred | Moderate |
| Hot chloride brine, crevices | Good | Preferred on cost |
| Seawater, general | Good (Grade 2 usually enough) | Good |
| Relative material cost | High (Pd content) | Lower |
| Strength level | ≈345 MPa | ≈483 MPa |
Both are ASTM B348. For oil and gas, NACE MR0175 / ISO 15156 lists Gr2, Gr7 and Gr12 with environmental limits attached. The limits in the standard decide suitability, not the grade name on its own.
| Form | Range | Condition | Tolerance |
|---|---|---|---|
| Ground round bar | Ø10–80 mm | Annealed | h8–h9 |
| Peeled / turned bar | Ø20–250 mm | Annealed | h9–h11 |
| Cut length | Up to 6,000 mm | As cut | ±1 mm |
Grade number follows product form, and that trips people up. A drawing that calls Grade 11 on a bar means Grade 7, because Grade 11 is the plate, sheet and strip specification for the same alloy. Order the bar grade for bar stock and save the argument at goods-in.
| Packing | Bundled on wooden skid with plastic sleeve; ISPM-15 case for small sizes |
| Stock sizes | on request |
| Lead time | on request |
| Minimum order | on request |
Is Grade 7 the same as Grade 11?
Both are Ti-0.2Pd. Grade 7 covers bar and billet, Grade 11 covers plate, sheet and strip. On a bar drawing, ask for Grade 7.
Can Grade 12 replace Grade 2 in seawater?
Grade 2 is usually adequate in flowing seawater. Grade 12 earns its price where crevices, deposits or higher temperature raise the risk, so describe the service before defaulting to the expensive grade.
Do you supply to NACE MR0175?
Yes, with a compliance statement against the applicable environmental limits and an MTC showing the required chemistry.
Tell us the medium, concentration, temperature and whether crevices exist. That picks the grade better than a drawing alone does.