Titanium electrode bar for EIGA and plasma atomization, 50-100 mm, turned and UT tested.
A powder atomizer melts a titanium electrode and breaks it into droplets. That electrode is a bar, and the powder inherits what the bar carries: oxygen, nitrogen, a porous centre, a segregated band. We supply electrode bar for EIGA, plasma and PREP machines in Grade 5 and Grade 23 ELI, 50–100 mm diameter, turned and ultrasonic tested.
| Grade | Typical powder | Bar standard | Watch |
|---|---|---|---|
| Grade 5 | SLM, EBM, DED | ASTM B348 | O ≤ 0.20%, Al/V uniform |
| Grade 23 ELI | Medical, aerospace | ASTM B348 / F136 | O ≤ 0.13%, Fe ≤ 0.25% |
| Grade 2 | CP-Ti powder | ASTM B348 | O ≤ 0.25%, low Fe |
| Ti-6242, others | Specialty | Quoted to drawing | Lot size and mill lead time |
| Item | Range | Note |
|---|---|---|
| Diameter | 50–100 mm | Matched to the electrode holder |
| Length | 500–3,000 mm | Cut to the furnace's usable length |
| Surface | Turned, peeled or ground | No alpha case, no rolled-in scale |
| Straightness | 0.5–1 mm/m | Tighter on request |
| Condition | Annealed | Stress relief on request |
Powder specifications such as ASTM F2924 and F3001 describe the powder. None of them describe the rod that made it. If the electrode has a porous centre, the atomizer finds out the expensive way: the pour gets unstable, satellites go up, oxygen drifts and the batch fails after the argon has been spent.
So the questions we get are about the rod. Heat number. Interstitial analysis with oxygen, nitrogen, hydrogen and iron reported separately. The ultrasonic result and the acceptance level it was judged against. Whether the surface was turned or just pickled. A certificate that says "conforms" is not enough for this customer; they want the numbers.
Diameter consistency matters more than the nominal size. A rod that tapers changes the melt rate and the arc stability, so we measure at both ends and the middle and put the readings on the report.
| Packing | Each bar sleeved, ends protected, ISPM-15 case, heat tag on the piece |
| Stock sizes | on request |
| Lead time | on request |
| Minimum order | on request |
Do you sell powder?
No. We supply the bar that goes into the atomizer. If you need powder, tell us the cut and the specification and we will say whether it is available through the atomizers we work with.
Which oxygen level should I specify?
Work back from the powder specification your customer gave you. Atomization adds little oxygen, but the rod sets the floor. For ELI powder, Grade 23 rod with O ≤ 0.13% and the interstitial numbers on the certificate.
Can you match an existing qualified rod?
Usually. Send the drawing and the acceptance criteria you already qualified. Matching an existing qualification is faster than starting from a generic standard.
Send grade, diameter, length, atomizer type, interstitial limits and UT level. If you have a rod specification already, send that instead.
Contact: Jessie