Grade 2 titanium plate (CP titanium, UNS R50400, W.Nr 3.7035, GB TA2) to ASTM B265, 0.5 mm to 100 mm thick and up to 2,000 mm wide. Grades 1, 3 and 4…
Grade 2 titanium plate (CP titanium, UNS R50400, W.Nr 3.7035, GB TA2) to ASTM B265, 0.5 mm to 100 mm thick and up to 2,000 mm wide. Grades 1, 3 and 4 run the same route at different oxygen levels, so one inquiry can cover a formed tank head and a heavy tube sheet. Common thicknesses are stocked and cut to size with a mill certificate. Part of our titanium plate and sheet range.
| Duty | Grade | Usual thickness | Note |
|---|---|---|---|
| Formed tank head | Grade 1 | 0.5–3 mm | Highest elongation |
| Welded shell, liner | Grade 2 | 2–12 mm | Standard weldable plate |
| Heat exchanger tube sheet | Grade 2 or 3 | 12–60 mm | Drilled on a bore pattern |
| Load-bearing bracket | Grade 4 | 3–20 mm | About 550 MPa, same corrosion behavior |
| Cover, duct, splash guard | Grade 2 | 0.8–3 mm | Light gauge, often bright rolled |
Minimums per ASTM B265 at room temperature: Grade 1 Rm 240 MPa, Grade 2 345, Grade 3 450, Grade 4 550. Grade 4 is the same metal with more oxygen, which buys about 200 MPa and costs formability. For strength at less thickness, see Grade 5; the grade chart covers the rest.
| Item | Range | Typical tolerance |
|---|---|---|
| Sheet thickness | 0.5–4.75 mm | Per ASTM B265, by width |
| Plate thickness | 4.75–100 mm | Per ASTM B265, by width |
| Width | Up to 2,000 mm | +5/0 mm, sheared edge |
| Length | Cut to order | ±2 mm on sawn ends |
| Squareness | Sheared or sawn | ±1 mm per 1,000 mm |
Plate thickness tolerance is not symmetric and it tightens as the width drops: the same nominal gauge is a different tolerance at 1,000 mm and at 2,000 mm. The measured range goes on the dimensional report, not a bare B265.
Pickled and descaled is the normal supply and the right face for welding: the acid takes the alpha case off and leaves a matte surface a pool will wet. Grinding is ordered where the face is a gasket or liner seal. Pickled keeps a slight profile and welds without more prep. Ground is flatter, removes thickness, and the gauge you receive is measured after grinding.
Cut edges come sheared, sawn or machined. A shear rolls the top face over and leaves a burr underneath; on 8 mm plate that suits weld prep and fails on a sealing face.
MTC to EN 10204 3.1 with heat number, chemistry, tensile and yield. PMI by XRF or OES on request, dimensional report with thickness and flatness readings, third-party inspection before shipment.
| Item | Detail |
|---|---|
| Packing | Wooden pallet, paper interleave, steel strapping; ISPM-15 case for thin sheet |
| Stock thicknesses | on request |
| Lead time | on request |
| Minimum order | on request |
Thin sheet is blocked flat, never stood on edge, and PE film goes on visible faces; under 0.5 mm the material is titanium strip and foil.
Thin sheet can be fused. Plate work should run ERTi-2 filler with argon on both sides, and the shield has to hold until the metal drops below about 400 °C, so a trailing shield usually comes into it.
It was pickled to remove the alpha case left by hot rolling. That is the normal supply condition and the right surface for welding and forming. Bright rolled sheet is available where the face shows.
Not on its own. A 2 mm sheet welded across a 1.5 m panel will bow, and clamping afterwards does not take it out. Back-step the sequence, hold the tacks until the root is in, and plan on leveling. Where flatness is functional, order stress-relieved plate.
Send grade, thickness, width, length, quantity, surface and edge condition. If the plate feeds a formed or welded part, add the process: it decides the temper and the flatness callout.
Contact: Jessie
Phone: +86-19539017809
E-mail: sales@gktitanium.com
Add: BLOCK A, HUIHANG PLAZA , HANGTUO ROAD, NATIONAL CIVIL AEROSPACE INDUSTRY BASE, Xi'an