Cut-to-Size Titanium Plate

Cut to size titanium plate from stock: sheared rectangles, sawn blocks, waterjet profiles or plasma blanks in Grades 1–5 and the corrosion grades,…

EMAIL

Cut to size titanium plate from stock: sheared rectangles, sawn blocks, waterjet profiles or plasma blanks in Grades 1–5 and the corrosion grades, 0.5 mm to 100 mm thick. Send a drawing or DXF; the reply carries a nested layout, a tolerance statement and a price for finished blanks rather than a full plate. Edges are deburred and parts ship in cutting sequence. Part of our titanium plate and sheet range.

Send Your DXF

Why Blanks

A 320 × 240 mm part out of a 1,000 × 2,000 mm plate leaves a lot of titanium on the floor, and offcut sells for far less than plate. Nesting and common-line cutting turn a plate price into a part price. The second reason is the edge. Shear leaves a straight edge with slight roll-over and a burr underneath: fine for weld prep on thin plate, wrong for a sealing face. Waterjet leaves a square, oxide-free edge with no heat-affected zone and a small taper on thick sections. Plasma is fast above 20 mm but leaves a nitride layer to grind before welding.

Cutting Processes

ProcessThicknessTypical toleranceEdgeUse for
Shear0.5–6 mm±0.5 mmStraight, slight roll-overRectangles, weld prep strips
Band saw3–100 mm±1 mmSawn, squareBlocks, thick plate, ring blanks
Waterjet0.5–100 mm±0.2 mmMatte, no HAZ, small taperProfiles, holes, weldable edges
Laser0.5–8 mm±0.1 mmThin oxide layerThin parts, many small features
Plasma3–60 mm±1 mmNitride layer, must be groundRough blanks, thick plate

Values are typical and confirmed on the drawing. Holes under about 1.5× the plate thickness are usually drilled rather than cut.

Nesting and Yield

Every cut quote is built on a layout, and the layout goes out with the price. The outside of a mill plate is not always sound, so we trim the edge before nesting and quote from the trimmed area. Where two parts share an edge, a common-line cut saves one kerf and one pass. The offcut comes back to you or stays with us as credit.

On a repeat part the layout stays on file, so the next order nests the same way and the price stops moving.

Dimensions and Tolerance

FeatureTypicalAvailable on request
Blank length and width±0.5 mm sheared, ±0.2 mm waterjet±0.1 mm, cut then milled
Squareness±1 mm per 1,000 mmMachined edge, ±0.2 mm
Hole position±0.3 mm waterjetDrilled on a pattern
FlatnessAs plate, checked before packingStress relief plus leveling
Edge finishDeburredMachined, radiused, weld prep

Cutting releases residual stress. On 3 mm plate that is a 0.5 mm bow over a metre, and it arrives after the cut, not before. Where flatness is functional, quote stress-relieved plate and a leveled blank, and expect one extra operation.

Packing and Marking

ItemDetail
CaseISPM-15 plywood case, parts separated by paper or foam, strapped so nothing moves
MarkingPart number and heat number on each piece, or neutral marking
SequencePacked in cutting or kitting order
WeightUp to 1,000 kg per case; heavier parts on a cradle
Lead timeon request
Minimum orderon request

FAQ

Can you cut from plate I supply?

Standard work is cut from our own stock, which keeps the heat number and the certificate chain in one place. Customer-supplied plate is handled case by case. on request

Why is a waterjet blank dearer than a sheared one?

Cutting speed and garnet. Waterjet removes material slowly and the abrasive is consumed, so price follows cut length, not area. On a rectangle the shear wins; on a profile with holes waterjet may be the only route.

Can you hold flatness after cutting?

Up to a point. Cutting relieves stress and thin plate bows. Where flatness matters we quote stress-relieved plate and a leveled blank, measure before packing, and put the figure on the report. Tolerance guide →

Quote

Send the DXF, grade, thickness, quantity and the tolerance you work to. Add the end use if the part is formed or welded: it decides the rolling direction and, on Grade 5, whether the plate needs stress relief first.

Send Your Requirement

Related

INQUIRY

CATEGORIES

CONTACT US

Contact: Jessie

Phone: +86-19539017809

E-mail: sales@gktitanium.com

Add: BLOCK A, HUIHANG PLAZA , HANGTUO ROAD, NATIONAL CIVIL AEROSPACE INDUSTRY BASE, Xi'an