Corrosion-Resistant Titanium Plate, Grade 7, 11 and 12

Titanium grade 12 plate (Ti-0.3Mo-0.8Ni, UNS R53400) is the Mo-Ni answer to crevice corrosion: about 483 MPa tensile, plus hot brine and wet chlorine…

EMAIL

Titanium grade 12 plate (Ti-0.3Mo-0.8Ni, UNS R53400) is the Mo-Ni answer to crevice corrosion: about 483 MPa tensile, plus hot brine and wet chlorine resistance that Grade 2 does not survive. For reducing acid, the answer is the palladium grades, Grade 7 plate or Grade 11 sheet, Ti-0.2Pd. All three run to ASTM B265, 0.5 mm to 50 mm.

Request a Quote

How the Grades Differ

Titanium works on an oxide film: stable in oxidizing acid, gone in reducing acid, and worst in a gasketed joint where the crevice keeps oxygen out while acid sits in it. Palladium in Grades 7 and 11 repairs that film where there is no oxygen. Grade 12 goes another way: molybdenum and nickel raise chloride and brine resistance at alloy cost close to Grade 2.

Each one has a wall. Grade 7 handles hydrochloric and sulfuric service that would eat Grade 2, and does nothing useful in hot brine. Grade 12 owns brine, wet chlorine and crevices, and will not hold in reducing acid.

Grade Comparison

PropertyGrade 7Grade 11Grade 12
AlloyTi-0.2PdTi-0.2PdTi-0.3Mo-0.8Ni
UNSR52400R52250R53400
AdditionPd 0.12–0.25%Pd 0.12–0.25%Mo and Ni
Rm / Rp0.2 (MPa, min)345 / 275345 / 275483 / 345
Cost driverPalladium, indexedPalladium, indexedAlloying, near Grade 2
Typical mediumReducing acidsReducing acids, sheetHot brine, crevices
Typical thickness0.5–50 mm0.5–4.75 mm0.5–50 mm

Values are B265 minimums. Grade 12 is stronger than Grade 2, so a thinner plate sometimes does the same job.

Choosing by Medium

ServiceFirst choiceWhy
Hydrochloric acid, dilute to moderateGrade 7Pd keeps the film repaired without oxygen
Sulfuric acid, reducingGrade 7Same mechanism, temperature dependent
Seawater, ambientGrade 2Film stable; alloy wasted
Hot brine, evaporator plateGrade 12Mo-Ni resists chloride pitting
Wet chlorine, hypochloriteGrade 12Better than Grade 2 under gaskets
Nitric acid, oxidizingGrade 2Film stable; no benefit from alloy

Concentration, temperature and whether oxygen is present decide between Pd and Mo-Ni more often than the acid name does. Send all three. Ambient service starts at Grade 2 titanium plate.

Fabrication

Grade 7 welds with ERTi-7 filler, Grade 12 with ERTi-12, full argon shielding, purge on the back side, no colour on the bead. A straw tint means oxygen went in and the film there is now Grade 2 at best. Grade 12 machines like a stronger Grade 2: sharp carbide, heavy feed, no dwell. Iron or copper pickup from a carbon steel brush destroys the film locally, so those plates get their own tooling.

Inspection and Documents

  • MTC to EN 10204 3.1 with chemistry including Pd, Mo and Ni
  • PMI on every plate where Pd content is critical; XRF reads Pd directly
  • Flatness and dimensional report; third-party inspection on request

Applications

Packing and Lead Time

ItemDetail
PackingWooden pallet, paper interleave, strapping; grade and heat number on each plate
Stock gradeson request
Lead timeon request
Price basisPd grades quoted against the palladium price of the day on request
Minimum orderon request

FAQ

Can Grade 12 replace Grade 7 in hydrochloric acid?

Usually not. Grade 12 is stronger in chlorides, hot brine and crevices, but in reducing acid the Pd couple keeps the film intact. An HCl vessel with tight joints usually ends up Grade 7 on the wetted surface.

Why does Pd plate price move between quotes?

Palladium is a large share of the material cost and trades daily. Gr7 and Gr11 are quoted against the metal price on the quote date, and the quote states how long the figure holds.

Is Grade 11 different from Grade 7?

Same alloy family, same Pd range. Grade 11 is the B265 designation for sheet and strip with tighter interstitial limits, so order it when the drawing says Grade 11, and Grade 7 for plate. Grade chart →

Quote

Send concentration, temperature, whether oxygen is present, thickness and quantity. We quote the grade we would use and the next one up.

Send Your Requirement