Titanium disc forging, blocks and step shafts to ASTM B381 in F-2, F-5 and F-23, to 3,000 kg (6,600 lb) per piece and 1,500 mm (59 in) across. These…
Titanium disc forging, blocks and step shafts to ASTM B381 in F-2, F-5 and F-23, to 3,000 kg (6,600 lb) per piece and 1,500 mm (59 in) across. These are thick sections, and the grain pattern has to run the way the load does, so flow direction is settled at drawing review.
A disc is upset: the billet is compressed on its axis, the section spreads, and the grain is pushed outward into the disc plane. A shaft is drawn the other way, with the section reduced along the axis until the grain forms longitudinal lines. A block sits between the two, cogged on one axis and left as a squared blank.
Each route leaves a different pattern, and the pattern should point where the load goes. The same shape machined from forged bar looks identical on the drawing. In service it is not: cutting across flow lines puts end grain at fillets and bores.
| Part | Forge route | Reduction | Grain flow |
|---|---|---|---|
| Disc, blank flange | Upset from cut billet | ≥3:1 | Radial, in the disc plane |
| Block, die block | Cogged, one axis | ≥3:1 | Along the long axis |
| Step shaft, stub axle | Drawn out on axis | ≥3:1 | Longitudinal, follows steps |
| Hub, boss, coupling | Upset and punched | ≥3:1 | Follows the outer contour |
Reduction is measured from billet cross-section to finished forging and written on the route card. A drawing that asks for 4:1 or 5:1 goes on a separate route. Where the drawing is silent, 3:1 is what we forge and report.
| Item | Range | Note |
|---|---|---|
| Disc diameter | ≤1,500 mm (59 in) | Thickness per drawing |
| Block diagonal | ≤1,500 mm (59 in) | Squared by milling on request |
| Step shaft | Length per drawing | End stock inside the allowance |
| Single piece weight | ≤3,000 kg (6,600 lb) | Under 500 kg cased |
| As-forged allowance | 3–5 mm per face and diameter | Restated at drawing review |
A thick part cannot be judged from its surface, so UT runs on a grid or a full scan to ASTM A388 or the level you nominate. We run it before rough turning where the geometry allows, so the probe travels on a turned face instead of on scale.
Tension tests come from a prolongation of the same lot. Hardness is checked across the section, because a 1,500 mm disc does not cool evenly: centre and rim can differ, and the drawing usually cares about one of them.
Every piece carries heat and lot numbers, plus a serial where the drawing requires one. The route card holds billet heat, reduction, forging temperatures and the heat treatment chart. See the inspection sequence →
| Item | Detail |
|---|---|
| Packing | Bolted to an ISPM-15 skid over 1,000 kg; smaller pieces under VCI film in a case |
| Forging lead time | on request |
| Rough machining | on request |
| Minimum order | on request |
Why not machine the disc from plate?
For a thin disc you can, and it is cheaper. For a thick section, plate gives no through-thickness flow and limited UT coverage, and most of what you buy turns into chips.
How do I know the forging ratio was met?
It is on the route card with billet size and finished section. A copy goes with the certificate when your quality plan asks for one.
Can you hold flatness after solution treating?
Not on as-forged faces. STA moves the part, which is why the allowance grows and the sequence runs rough machine, stress relieve, finish. That sequence is cheaper settled before release.
Send the drawing, grade, quantity, load direction if it is known, and the UT level. If the part is machined in one setup, tell us the datum, because the allowance has to survive it.